Deox Sterling Non-Tarnishing Silver

Home / Publications / Online Library / Deox Sterling Non-Tarnishing Silver

Deox Sterling Non-Tarnishing Silver

 

 

General Alloy Composition

92.5% silver, copper, tin, proprietary trace elements

 

 

Suitable for

Casting

 

 

Melting Temperature Range

Solidus: 1558°F (848°C)

Liquidus: 1675°F (913°C)

 

 

Hardness (As-Cast) (HV)

• Dwell for 15-20 minutes (after casting, before quenching): 155 HV

• No dwell (less than 3 minutes): 120 HV

 

 

Hardness (70% Cold-Work) (HV)

• Fully annealed (dead-soft) before cold working: N/A

• As-cast before cold working: N/A

• Torch annealed before cold working: N/A

 

 

Hardness (Age-Hardened) (HV)

• Two-step age hardness: N/A

• Single-step age hardness: N/A

 

 

Available Forms

Casting grain

 

 

Fusing Possible

No

 

 

Welding Possible

Yes

 

 

Quenching Guidelines

At 800°F to 600°F

 

 

Special Tips for Working with Alloy

N/A

 

 

Contact

Precious Metals West/Fine Gold

1-213-689-4872

daniel@pmwest.us

preciousmetalswest.com